Ragar niobium mai faɗaɗɗe mai rufin platinum
Tuntuɓe mu don samun sabon farashi
Ragar niobium mai rufin platinum anode ce mara narkewa da aka yi daga farantin niobium mai faɗaɗɗe mai shafin platinum, wadda aka ƙera don kwamin shafa ƙarfe da lantarki (electroplating) mai sauri da yawan current density.
- Tushe (substrate): farantin niobium (Nb) mai faɗaɗɗe
- Shafi: platinum, na yau da kullum 2–5 µm, har zuwa 20 µm don aiki mai tsanani
- Yawan current (current density): har zuwa 100 A/dm²
- Iyakar pH: 0–11
- Iyakokin aiki: fluoride ƙasa da 500 mg/L, zafi ƙasa da 80 ℃
- Siffofi: ƙarancin juriyar wutar lantarki, tsari mai tauri, ba ya buƙatar gyara akai-akai, ana iya sake shafa masa platinum
- Amfani: shafa ƙafafun mota na aluminum, shafa ƙarafa masu daraja da samar da perchlorate
Bayani
Ragar niobium mai rufin platinum anode ce mara narkewa da aka yi daga farantin niobium mai faɗaɗɗe da aka shafa wa layin platinum. Niobium yana ba da tushe mai ƙarfi, mai jure lalacewa (corrosion) sosai kuma mai gudanar da wutar lantarki, yayin da saman platinum ke ɗaukar current. An ƙera wannan haɗin don kwamin shafa ƙarfe masu sauri da ke aiki da yawan current density.
Idan aka kwatanta da ragar titanium mai shafin platinum, anode ta niobium mai shafin platinum na iya ɗaukar ƙarin current a kowane fili na saman kuma tana daɗewa a yanayi mai tsanani, wanda ke rage jimillar kuɗin aiki a layukan shafa ƙarfe masu nauyi.
Fa'idodi
- Ana iya samar da anodes masu siffa mai sarƙaƙiya
- Aiki mai sauƙi ba tare da gyara akai-akai ba
- Ƙarancin juriyar wutar lantarki
- Jure lalacewa (corrosion) matuƙa
- Ta dace da electrolytes masu ɗauke da fluoride
- Daɗewar amfani a yawan current density
- Tsari mai tauri da ba ya karkacewa
- Ana iya sake shafa wa tushen niobium platinum
Amfani
- Shafa ƙarfe da lantarki (electroplating) mai sauri da yawan current density
- Shafa ƙafafun mota na aluminum
- Shafa ƙarafa masu daraja
- Samar da perchlorate
Bayanan fasaha
- Tushe (substrate): farantin niobium mai faɗaɗɗe (Nb)
- Shafi: platinum (Pt)
- Kaurin layin platinum: na yau da kullum 2–5 µm; har zuwa 20 µm don aiki mafi tsanani
- Yawan current (current density): 100 A/dm² a mafi yawa
- Iyakar pH: 0–11
Bayanan aiki da ke ƙasa suna ba da yawan platinum, yawan fluoride da aka yarda da shi da iyakar zafi, da lokacin aikin da ake tsammani.
| 基体金属 Ƙarfen tushe: |
Nb | 涂层氧化物 Oxide na shafi: |
Pt |
| 电流密度范围 Iyakar current density: |
ƙasa da 10000A/M2 | 铂金含量 Yawan platinum: |
≥10g/m2 |
| 氟离子含量 Yawan fluoride: |
ƙasa da 500mg/L | 温度范围 Iyakar zafi: |
ƙasa da 80℃ |
| 使用时间 Lokacin amfani: |
fiye da 10watanni | 涂层厚度 Kaurin shafi |
fiye da 3um |

Baya ga raga, ana iya yin anodes masu tushen niobium a matsayin faranti, sanda, waya da bututu. Ana iya daidaita kaurin shafi da siffar anode da zanen kwaminku (cell).
Kayayyaki masu alaƙa
- Ragar titanium saƙaƙƙiya mai jure lalacewa (corrosion)
- Ragar zirconium don vacuum da zafi mai yawa
- Ragar wayar titanium
- Ragar aluminum mai faɗaɗɗe
- Ragar wayar iron-chrome-aluminum (FeCrAl)
- Zanen ragar waya saƙaƙƙe na ƙarfe mara tsatsa 304 316
Aiko mana da zanen anode ɗinku, sinadaran kwamin da buƙatun current, kuma za mu ba ku farashin anode da ta dace.
Daga masana'antarmu
- An ƙera a masana'antarmu mai faɗin 5,000 m² a gundumar Anping, Hebei, cibiyar ragar waya ta ƙasar Sin. An kafa kamfaninmu a 2007.
- Muna fitar da kaya zuwa Yammacin Afirka, Gabashin Afirka, Jamus da sauran ƙasashen Turai, da Ostareliya.
- Aiko mana da kayan, girman raga da yawan da kuke buƙata ta WhatsApp don samun farashi. +86-18732863999